Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PAI Compoceran H901-2D ARAKAWA JAPAN
--
thin film
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Supplementary Information | Test Condition | Test Method | ARAKAWA JAPAN/Compoceran H901-2D |
|---|---|---|---|
| Silicon dioxide (SiO?) content | 2.0 wt% | ||
| solvent | DMAc |
| Uncured Properties | Test Condition | Test Method | ARAKAWA JAPAN/Compoceran H901-2D |
|---|---|---|---|
| Solid content | 30 % | ||
| viscosity | 25°C | 4.0 Pa·s |
| Physical properties | Test Condition | Test Method | ARAKAWA JAPAN/Compoceran H901-2D |
|---|---|---|---|
| FunctionalGroup-Silica | 4.00 |