Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP Copolymer MOSTEN MT 812 Unipetrol RPA, s.r.o.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Unipetrol RPA, s.r.o./MOSTEN MT 812 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179 | 6.0 kJ/m² |
-20°C | ISO 179 | 1.2 kJ/m² |
Mechanical properties | Test Condition | Test Method | Unipetrol RPA, s.r.o./MOSTEN MT 812 |
---|---|---|---|
Tensile strain | 断裂 | ISO 527-2 | >250 % |
tensile strength | 屈服 | ISO 527-2 | 26.0 MPa |
Flexural modulus | ISO 178 | 1050 MPa |
physical property | Test Condition | Test Method | Unipetrol RPA, s.r.o./MOSTEN MT 812 |
---|---|---|---|
melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 12 g/10min |
Thermal performance | Test Condition | Test Method | Unipetrol RPA, s.r.o./MOSTEN MT 812 |
---|---|---|---|
vicat | ISO 306 | 132 °C | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 48.0 °C |
Contact Us
Get App