Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPO PC180X-701 SABIC INNOVATIVE US
NORYL™
Office supplies
Flame retardant, Flame retardant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/PC180X-701 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa | ASTM D-648 | 80 °C |
| 0.45MPa | ASTM D-648 | 90 °C | |
| Long term use temperature | 电气 | UL 746B | 50 °C |
| 含冲击 | UL 746B | 50 °C | |
| 无冲击 | UL 746B | 50 °C | |
| Volume resistivity | ASTM D-257 | 3.0×10 Ω.cm |
| mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/PC180X-701 |
|---|---|---|---|
| Bending modulus | 6.4mm | ASTM D-790 | 2205 Mpa |
| bending strength | 6.4mm | ASTM D-790 | 80 Mpa |
| Impact strength of cantilever beam gap | 23°C | ASTM D-256 | 309 J/m |
| Rockwell hardness | ASTM D-785 | 117 | |
| tensile strength | 屈伏点,3.2mm | ASTM D-638 | 55 Mpa |
| Break点,3.2mm | ASTM D-638 | 22 Mpa |
| Electrical performance | Test Condition | Test Method | SABIC INNOVATIVE US/PC180X-701 |
|---|---|---|---|
| Dielectric constant | 1MHz | ASTM D-150 | 2.53 |
| Surface resistivity | ASTM D-257 | 1.0×10 Ω.cm |
| Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/PC180X-701 |
|---|---|---|---|
| Shrinkage rate | 3.2mm | ASTM D-955 | 5-7 |