Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

EPDM S552 SK KOREA
SUPRENE®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | SK KOREA/S552 |
---|---|---|---|
Shore hardness | ShoreD | ASTM D2240 | 59 |
Supplementary Information | Test Condition | Test Method | SK KOREA/S552 |
---|---|---|---|
HalogenAcidGasEvolution | IEC 60754-1 | 0.0 % |
thermal performance | Test Condition | Test Method | SK KOREA/S552 |
---|---|---|---|
Hot pressing test | 90°C | IEC 60811-3-1 | 35 % |
mechanical properties | Test Condition | Test Method | SK KOREA/S552 |
---|---|---|---|
Elongation at Break | after7days,inIRM903Oil:23°C | 160 % | |
after4hours,inSAE20Oil:70°C | 180 % | ||
after7days,inIRM902Oil:23°C | 220 % | ||
after4hours,inIRM902Oil:70°C | 210 % | ||
Tensile strain | Break | IEC 60811-1-1 | 200 % |
Break3 | IEC 60811-1-2 | 170 % | |
Break2 | IEC 60811-1-2 | 170 % | |
tensile strength | after4hours,inIRM902Oil:70°C | 13.5 Mpa | |
--2 | IEC 60811-1-2 | 15.0 Mpa | |
--3 | IEC 60811-1-2 | 17.0 Mpa | |
-- | IEC 60811-1-1 | 14.0 Mpa | |
after7days,inIRM902Oil:23°C | 14.5 Mpa | ||
after4hours,inSAE20Oil:70°C | 13.5 Mpa | ||
after7days,inIRM903Oil:23°C | 12.5 Mpa |
Physical properties | Test Condition | Test Method | SK KOREA/S552 |
---|---|---|---|
melt mass-flow rate | 150°C/21.6kg | ISO 1133 | 5.5 g/10min |
flammability | Test Condition | Test Method | SK KOREA/S552 |
---|---|---|---|
Acid gas release | IEC 60754-2 | 4.00 µS/cm | |
pH | IEC 60754-2 | 5.70 | |
Combustion temperature index | ISO 4589-3 | 280 °C | |
Extreme Oxygen Index | ISO 4589-2 | 36 % | |
smoke density | Non-flamingmode | ASTME662 | <140 Ds |
Flamingmode | ASTME662 | <60 Ds | |
toxicity | NES713 | 0.600 |
aging | Test Condition | Test Method | SK KOREA/S552 |
---|---|---|---|
Change rate of tensile strength in air | 70°C,4hr,inSAE20Oil | -5.0 % | |
70°C,4hr,inIRM902Oil | -5.0 % | ||
23°C,168hr,inIRM902Oil | 5.0 % | ||
110°C,168hr | 20 % | ||
70°C,168hr,inWater | BS646999.1 | -12 % | |
23°C,168hr,inIRM903Oil | -10 % | ||
100°C,168hr | 5.0 % | ||
Tensile stress change rate | 70°C,168hr,inWater,Break | BS646999.1 | -5.0 % |
23°C,168hr,inIRM903Oil,Break | -20 % | ||
23°C,168hr,inIRM902Oil,Break | 10 % | ||
110°C,168hr,Break | -15 % | ||
70°C,4hr,inIRM902Oil,Break | 5.0 % | ||
70°C,4hr,inSAE20Oil,Break | -10 % | ||
100°C,168hr,Break | -15 % |
elastomer | Test Condition | Test Method | SK KOREA/S552 |
---|---|---|---|
tear strength | BS646999.1 | 8.00 kN/m |