PUR-Ester/PPDI LFP 1950A CHEMTURU USA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | CHEMTURU USA/ LFP 1950A |
---|---|---|---|
Dynamic Properties | TangentDelta:30°C | 0.0180 | |
StorageModulus:150°C | 2.42E+08 dynes/cm² | ||
TangentDelta:150°C | 0.0140 | ||
StorageModulus:30°C | 3.14E+08 dynes/cm² |
hardness | Test Condition | Test Method | CHEMTURU USA/ LFP 1950A |
---|---|---|---|
Shore hardness | 邵氏A | ASTM D2240 | 93to95 |
Mechanical properties | Test Condition | Test Method | CHEMTURU USA/ LFP 1950A |
---|---|---|---|
compressive strength | 20%应变 | ASTM D695 | 9.31 MPa |
10%应变 | ASTM D695 | 4.83 MPa | |
25%应变 | ASTM D695 | 12.1 MPa | |
5%应变 | ASTM D695 | 2.48 MPa | |
15%应变 | ASTM D695 | 6.89 MPa |
thermosetting | Test Condition | Test Method | CHEMTURU USA/ LFP 1950A |
---|---|---|---|
STORAGE STABILITY | 6.0 min | ||
Post curing time | 116°C | 16 hr | |
stripping time | >60 min |
elastomer | Test Condition | Test Method | CHEMTURU USA/ LFP 1950A |
---|---|---|---|
compression set | 100°C,22hr | ASTM D395B | 50 % |
elongation | 断裂 | ASTM D412 | 650 % |
tear strength | 开裂 | ASTM D470 | 28 kN/m |
Shore hardness | ASTM D2632 | 57 % | |
tensile strength | ASTM D412 | 48.3 MPa | |
compression set | 70°C,22hr | ASTM D395B | 35 % |
tensile strength | 100%应变 | ASTM D412 | 9.65 MPa |
300%应变 | ASTM D412 | 13.8 MPa |
physical property | Test Condition | Test Method | CHEMTURU USA/ LFP 1950A |
---|---|---|---|
density | ASTM D792 | 1.19 g/cm³ |