Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

HDPE C-220-N Spain Repsol
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic performance | Test Condition | Test Method | Spain Repsol/C-220-N |
---|---|---|---|
density | ASTM D-1505 | 0.952 g/m | |
melt mass-flow rate | 190℃/2.16 kg | ASTM D-1238 | 0.6 g/10min |
Mechanical properties | Test Condition | Test Method | Spain Repsol/C-220-N |
---|---|---|---|
Environmental stress cracking resistance | 10% Antarox CO-630,F0 | ASTM D-1693 | >1000 hr |
elongation | 断裂 | ASTM D-638 | 800 % |
vicat | ASTM D-1525 | 125 ℃ | |
tensile strength | 断裂 | ASTM D-638 | 27 MPa |
Electrical performance | Test Condition | Test Method | Spain Repsol/C-220-N |
---|---|---|---|
dielectric constant | 1E+6Hz | ASTM D-150 | 2.7 |
Dissipation Factor | 1E+6Hz | ASTM D-150 | 0.005 |
Thermal performance | Test Condition | Test Method | Spain Repsol/C-220-N |
---|---|---|---|
Melt Temperature | 190-220 ℃ |
Contact Us
Get App
Top