Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

SPS EA522 DUPONT-DOW US
--
--
Glass fiber reinforced、Filler/fiberglass reinfor、Fill 22% of weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic performance | Test Condition | Test Method | DUPONT-DOW US/EA522 |
---|---|---|---|
Water absorption rate | Stauration,23℃ | ISO 62 | 0.070 % |
density | ISO 1183/B | 1.32 g/cm |
Mechanical properties | Test Condition | Test Method | DUPONT-DOW US/EA522 |
---|---|---|---|
Impact strength of cantilever beam gap | ISO 180 | 10.00 KJ/m | |
Tensile stress | 屈服 | ISO 527-2 | 95.0 Mpa |
bending strength | ISO 178 | 150 Mpa | |
Flexural modulus | ISO 178 | 7600 Mpa | |
Suspended wall beam without notch impact strength | ISO 180 | 45.0 KJ/m | |
fracture strain | ISO 527-2 | 2.3 % | |
Impact strength of simply supported beam without notch | ISO 179 | 35.0 KJ/m | |
Charpy Notched Impact Strength | ISO 179 | 8.00 KJ/m |
Electrical performance | Test Condition | Test Method | DUPONT-DOW US/EA522 |
---|---|---|---|
dielectric constant | IEC 60250 | 3.000 | |
Volume resistivity | IEC 60093 | 1.8E+20 ohm.cm | |
Dielectric loss | IEC 60250 | 0.00100 |
physical property | Test Condition | Test Method | DUPONT-DOW US/EA522 |
---|---|---|---|
Shrinkage rate | Flow | ISO 294-4 | 0.20-0.40 % |
Across Flow | ISO 294-4 | 0.50-0.90 % |
Thermal performance | Test Condition | Test Method | DUPONT-DOW US/EA522 |
---|---|---|---|
vicat | ISO 306 | 255 °C | |
UL flame retardant rating | 2.00mm | UL 94 | V-2 |
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 255 °C |
RTI Str | 1.50mm | UL 746 | 120 °C |
RTI Imp | 1.50mm | UL 746 | 120 °C |
Heat distortion temperature | 1.80MPa,未退火,HDT | ISO 75-2/A | 210 °C |
UL flame retardant rating | 1.50mm | UL 94 | V-1 |
RTI Elec | 1.50mm | UL 746 | 125 °C |
Contact Us