Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPE TM3MED KRAIBURG TPE GERMANY
THERMOLAST® K
medicine、pipeline、packing、Valve components
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Elastomers Properties | Test Condition | Test Method | KRAIBURG TPE GERMANY/TM3MED |
---|---|---|---|
Compression Set | 100°C,24hr | ISO815 | 47 % |
23°C,72hr | ISO815 | 15 % | |
70°C,24hr | ISO815 | 28 % | |
Tensile Stress | 屈服 | ISO37 | 6.50 Mpa |
Tensile Elongation | 断裂 | ISO37 | 750 % |
Tearing Strength | ISO34-1 | 10 kN/m |
Hardness | Test Condition | Test Method | KRAIBURG TPE GERMANY/TM3MED |
---|---|---|---|
Shore Hardness | 邵氏A | ISO7619 | 27 |
Contact Us
Get App
Top