| mechanical properties | Test Condition | Test Method | DSM HOLAND/CX33F BK |
|---|---|---|---|
| tensile strength | Break | ISO 527-2 | 275 Mpa |
| Tensile modulus | ISO 527-2 | 17000 Mpa | |
| Tensile strain | Break | ISO 527-2 | 2.3 % |
| Physical properties | Test Condition | Test Method | DSM HOLAND/CX33F BK |
| Spiral flow length | 6.50 CM | ||
| thermal performance | Test Condition | Test Method | DSM HOLAND/CX33F BK |
| Glass transition temperature | ASTM D5026/D7028 | 130 °C | |
| Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 290 °C |
| Melting temperature | ISO 11357-3 | 315 °C |