PC/ABS FR3000 703003 COVESTRO GERMANY
Bayblend® 
Electrical field、Electronic field、Household appliances、Household appliances、Automotive sector
Flame retardant、UV resistance、High mobility
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodCOVESTRO GERMANY/FR3000 703003
Impact strength of cantilever beam gap23°CISO 180/A30 kJ/m²
Mechanical propertiesTest ConditionTest MethodCOVESTRO GERMANY/FR3000 703003
tensile strength 屈服, 23°CISO 527-2/5064.0 Mpa
Tensile modulus23°CISO 527-2/12650 Mpa
Nominal tensile fracture strain23°CISO 527-2/5040 %
Tensile strain屈服, 23°CISO 527-2/503.9 %
Electrical performanceTest ConditionTest MethodCOVESTRO GERMANY/FR3000 703003
relative permittivity23°C, 1 MHzIEC 602502.90
Volume resistivity23°CIEC 600931.0E+16 ohms·cm
relative permittivity23°C, 100 HzIEC 602503.00
Surface ResistivityIEC 600931.0E+16 ohms
flammabilityTest ConditionTest MethodCOVESTRO GERMANY/FR3000 703003
UL flame retardant rating2.0 mmUL 945VB
1.5 mmUL 94V-0
Limiting Oxygen IndexISO 4589-234 %
Filling analysisTest ConditionTest MethodCOVESTRO GERMANY/FR3000 703003
ISO 9660PC+ABS-FR(40)
melt viscosity240°CISO 11443-A150 Pa·s
physical property Test ConditionTest MethodCOVESTRO GERMANY/FR3000 703003
Shrinkage rate流量ISO 25770.40 - 0.60 %
density23°CISO 11831.18 g/cm³
Water absorption rate平衡, 23°C, 50% RHISO 620.10 %
Melt volume flow rate240°C/5.0 kgISO 113320.0 cm3/10min
Shrinkage rate横向流量ISO 25770.40 - 0.60 %
Water absorption rate饱和, 23°CISO 620.40 %
Thermal performanceTest ConditionTest MethodCOVESTRO GERMANY/FR3000 703003
Heat distortion temperature0.45 MPa, 未退火,HDTISO 75-2/B95.0 °C
vicatISO 306/B120103 °C
Heat distortion temperature1.8 MPa, 未退火,HDTISO 75-2/A85.0 °C
injectionTest ConditionTest MethodCOVESTRO GERMANY/FR3000 703003
Suggested maximum moisture content< 0.020 %
Drying time - Dry Air Dryer4.0 hr
Temperature in the middle of the barrel225 to 235 °C
Temperature at the rear of the barrel220 to 230 °C
Processing (melt) temperature240 to 270 °C
Exhaust hole depth0.025 to 0.075 mm
Suggested injection volume30 to 70 %
Temperature at the front of the material cylinder230 to 240 °C
Back pressure5.00 to 15.0 Mpa
Drying Temperature - Dry Air Dryer80 °C
Temperature60 to 90 °C
Spray nozzle temperature255 to 265 °C