SEBS 7125 KURARAY JAPAN
SEPTON™
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodKURARAY JAPAN/7125
Shore hardnessShoreAISO 86864
thermal performanceTest ConditionTest MethodKURARAY JAPAN/7125
Dissipation factorTangent-5 °C
Glass transition temperatureDSC-15.0 °C
Physical propertiesTest ConditionTest MethodKURARAY JAPAN/7125
melt mass-flow rate190°C/2.16kgASTM D12380.70 g/10min
230°C/2.16kgASTM D12384.0 g/10min
StyreneContentASTM D123820.0 wt%
Solution viscosity20wt%TolueneSolution:30°C55 mPa·s
30wt%TolueneSolution:30°C350 mPa·s
elastomerTest ConditionTest MethodKURARAY JAPAN/7125
elongationBreakISO 37680 %
tensile strength300%StrainISO 372.70 Mpa
YieldISO 377.10 Mpa
100%StrainISO 371.70 Mpa