Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA66 22HSP BK ASCEND USA
Vydyne®
Industrial applications,Electrical applications,Automotive Applications,Industrial machinery,Fitness equipment,Injection molding applications with basic engineer
Chemical resistance,High rigidity,wear resistant,Oil resistant,high strength,Thermal stability,High toughness,High liquidity,toughness,Chemical resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | ASCEND USA/22HSP BK |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa | ISO 75 | 200 °C |
| 1.82MPa | ISO 75 | 70 °C | |
| Melting temperature | ISO 3146 | 260 °C | |
| UL flame retardant rating | UL 94 | V-2 |
| mechanical properties | Test Condition | Test Method | ASCEND USA/22HSP BK |
|---|---|---|---|
| Bending modulus | ISO 178 | 2900 Mpa | |
| bending strength | ISO 178 | 35 Mpa | |
| elongation | Break | ISO 527 | 40 % |
| Impact strength of simply supported beam without notch | 23℃ | ISO 179 | 6.6 kJ/m² |
| -30℃ | ISO 179 | 5.3 kJ/m² | |
| Tensile modulus | ISO 527 | 3000 Mpa | |
| tensile strength | Yield | ISO 527 | 83 Mpa |
| Electrical performance | Test Condition | Test Method | ASCEND USA/22HSP BK |
|---|---|---|---|
| Dielectric strength | IEC 60243 | 20 KV/mm | |
| Volume resistivity | IEC 60093 | 4 ohm-cm×1015 |
| Physical properties | Test Condition | Test Method | ASCEND USA/22HSP BK |
|---|---|---|---|
| density | ISO 1183 | 1.14 g/cm³ | |
| Shrinkage rate | 2mm,平行 | ISO 294-4 | 1.4 % |
| 2mm,垂直 | ISO 294-4 | 1.6 % | |
| Water absorption rate | 23℃,24hrs | ISO 62 | 1.1 % |
| 23℃,50%湿度 | ISO 62 | 2.4 % |