Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPV 101-80 SHANGHAI LINGEN
--
packing,Wire and cable applications,pipeline,currency
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | SHANGHAI LINGEN/101-80 |
|---|---|---|---|
| Shore hardness | ShoreA,15Sec | ASTM D2240 | 80 |
| thermal performance | Test Condition | Test Method | SHANGHAI LINGEN/101-80 |
|---|---|---|---|
| Brittle temperature | ASTM D746 | -60.0 °C |
| aging | Test Condition | Test Method | SHANGHAI LINGEN/101-80 |
|---|---|---|---|
| Change rate of tensile strength in air | 150°C,168hr | 0.0 % | |
| Change rate of ultimate elongation in air | 150°C,168hr | -15 % |
| elastomer | Test Condition | Test Method | SHANGHAI LINGEN/101-80 |
|---|---|---|---|
| elongation | Break | ASTM D412 | 420 % |
| Permanent compression deformation | 120°C,22hr | ASTM D395 | 56 % |
| 70°C,22hr | ASTM D395 | 36 % | |
| 23°C,22hr | ASTM D395 | 25 % | |
| Stretch permanent deformation | ASTM D412 | 15 % | |
| tear strength | ASTM D624 | 42.0 kN/m | |
| tensile strength | 100%Strain | ASTM D412 | 4.90 Mpa |
| Yield | ASTM D412 | 10.8 Mpa |