Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
ABS 711 Kumho Sunny
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Basic performanceTest ConditionTest MethodKumho Sunny/711
melt mass-flow rate200℃×21.6kgASTM D-123845 g/10min
density23℃ASTM D-7921.04 g/cm3
melt mass-flow rate200℃×5kgASTM D-12383.6 g/10min
220℃×10kgASTM D-123833 g/10min
Mechanical propertiesTest ConditionTest MethodKumho Sunny/711
elongation at break23℃ASTM D-63830 %
Impact strength of cantilever beam gap1/8in(3.2mm).23℃ASTM D-25630 kg.cm/cm
tensile strength 23℃ASTM D-638450 Kg/cm2
Rockwell hardnessR SCALEASTM D-785105 R
Flexural modulus23℃ASTM D-79022000 Kg/cm2
bending strength23℃ASTM D-790650 Kg/cm2
Impact strength of cantilever beam gap1/4in(6.4mm).23℃ASTM D-25626 kg.cm/cm
physical property Test ConditionTest MethodKumho Sunny/711
Shrinkage rateASTM D-9550.4~0.7 %
Thermal performanceTest ConditionTest MethodKumho Sunny/711
Heat distortion temperature6.4mm 18.6kg/cm2 Annealed,HDTASTM D 64897(207) ℃(℉)
combustibilityUL 94相当HB CLASS
Heat distortion temperature6.4mm 18.6kg/cm2 Unannealed,HDTASTM D-64885(185) ℃(℉)
vicatASTM D-152596(205) ℃(℉)