PA66 A3 GF 60 1 AKRO-PLASTIC GERMANY
AKROMID®
Industrial applications、Automotive sector、Engineering accessories
Glass fiber reinforced、Thermal stability、high strength、High rigidity
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 60 1 |
---|---|---|---|
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 100 kJ/m² |
-30°C | ISO 179/1eU | 97 kJ/m² |
hardness | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 60 1 |
---|---|---|---|
ball-indentation hardness | H961/30 | ISO 2039-1 | 330 Mpa |
Supplementary Information | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 60 1 |
---|---|---|---|
ReinforcementContent | ISO 1172 | 60 % |
Mechanical properties | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 60 1 |
---|---|---|---|
Tensile modulus | ISO 527-2/1 | 20500 Mpa | |
tensile strength | 断裂 | ISO 527-2/5 | 260 Mpa |
bending strength | ISO 178 | 400 Mpa | |
Flexural modulus | ISO 178 | 19800 Mpa | |
Tensile strain | 断裂 | ISO 527-2/5 | 2.0 % |
Electrical performance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 60 1 |
---|---|---|---|
Volume resistivity | IEC 60093 | 1E+13 ohms·cm | |
Surface Resistivity | IEC 60093 | 1E+12 ohms | |
Compared to the Leakage Tracking Index (CTI) | 解决方案A | IEC 60112 | PLC 0 |
flammability | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 60 1 |
---|---|---|---|
burning rate | 1.00mm | FMVSS302 | <100 mm/min |
Burning wire flammability index | 1.6mm | IEC 60695-2-12 | 650 °C |
UL flame retardant rating | 0.8mm | UL 94 | HB |
physical property | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 60 1 |
---|---|---|---|
Shrinkage rate | TD | ISO 294-4 | 0.80 % |
MD | ISO 294-4 | 0.40 % | |
moisture absorption | 70°C,62%RH | ISO 1110 | 1.0to1.2 % |
spiral flow length | 内部方法 | 53.0 CM | |
Water absorption rate | 饱和,23°C | ISO 62 | 3.2to3.7 % |
Thermal performance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 60 1 |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 260 °C |
melting temperature | DIN EN11357-1 | 262 °C | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 260 °C |
8.0MPa,未退火,HDT | ISO 75-2/C | 235 °C |