Epoxy Magnobond 8007 Magnolia Plastics, Inc.
--
adhesive
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Electrical performance | Test Condition | Test Method | Magnolia Plastics, Inc./Magnobond 8007 |
---|---|---|---|
Volume resistivity | ASTM D257 | 6.6E-04 ohms·cm |
thermosetting | Test Condition | Test Method | Magnolia Plastics, Inc./Magnobond 8007 |
---|---|---|---|
shelf-life | -40°C | 52 wk | |
stripping time | 79°C | 60to180 min | |
Thermosetting mixed viscosity | ASTM D2393 | 194000 cP |
physical property | Test Condition | Test Method | Magnolia Plastics, Inc./Magnobond 8007 |
---|---|---|---|
density | ASTM D792 | 2.79 g/cm³ |