Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA66 A218V30 BK SOLVAY FRANCE
TECHNYL®
--
Filler: Glass fiber reinf,30%,Filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | SOLVAY FRANCE/A218V30 BK |
---|---|---|---|
Ball Pressure Test | 222.76to370.34 MPa |
thermal performance | Test Condition | Test Method | SOLVAY FRANCE/A218V30 BK |
---|---|---|---|
1.8MPa, unannealed | °C | 230to250 | |
8.0Mpa, unannealed | °C | 65to220 | |
Continuous use temperature | °C | 110to220 | |
flow | mm/mm/°C | 142.2E-5-203.2E-5 | |
Melting temperature | °C | 260 | |
transverse | mm/mm/°C | 68.6E-5-127.0E-5 |
mechanical properties | Test Condition | Test Method | SOLVAY FRANCE/A218V30 BK |
---|---|---|---|
Tensile modulus | 23℃ | 8206.9to28000.0 MPa | |
Tensile strain | Break,23℃ | % | 1.9to3.1 |
tensile strength | Break,23℃ | 144.83to292.41 MPa |
Electrical performance | Test Condition | Test Method | SOLVAY FRANCE/A218V30 BK |
---|---|---|---|
Dielectric strength | 23℃ | V/mil | 840 |
Volume resistivity | 23℃ | ohms·cm | 1.0E+12-1.0E+14 |
Physical properties | Test Condition | Test Method | SOLVAY FRANCE/A218V30 BK |
---|---|---|---|
Balance, 23 ℃, 50% RH | % | 1.2to1.5 | |
Saturation, 23 ℃ | % | 3.5to5.0 | |
Shrinkage rate | 23℃ | % | 0.10-0.31 |
impact performance | Test Condition | Test Method | SOLVAY FRANCE/A218V30 BK |
---|---|---|---|
Impact strength of simply supported beam without notch | 23℃ | kJ/m² | 11.143to19.964 |