| Basic Performance | Test Condition | Test Method | INEOS STYRO THAILAND/Novodur Ultra 4000PG |
|---|---|---|---|
| density | ISO 1183 | 1.05 | |
| Melt Volume Flow Rate (MVR) | 220℃,10kg | ISO 1133 | 7.00 CM |
| thermal performance | Test Condition | Test Method | INEOS STYRO THAILAND/Novodur Ultra 4000PG |
|---|---|---|---|
| Combustibility | 1.60mm | UL 94 | HB |
| Hot deformation temperature | 1.80MPa,Unannealed | ISO 75A-1 | 98.0 °C |
| 0.45MPa,Unannealed | ISO 75B-1 | 103 °C | |
| Linear coefficient of thermal expansion | 23℃-50℃ | ISO 11359-1 | 0.000090 cm/cm℃ |
| Vicat softening temperature | 50℃/h 50N | ISO 306 | 107 °C |
| mechanical properties | Test Condition | Test Method | INEOS STYRO THAILAND/Novodur Ultra 4000PG |
|---|---|---|---|
| Bending modulus | 23℃ | ISO 178 | 2350 Mpa |
| bending strength | 23℃ | ISO 178 | 73.0 Mpa |
| Charpy Notched Impact Strength | 23℃ | ISO 179/1eA | 20.0 KJ/m |
| -30℃ | ISO 179/1eA | 10.00 KJ/m | |
| Fracture strain | 23℃ | ISO 527-1 | 15 % |
| Impact strength of cantilever beam gap | 23℃ | ISO 180/1A | 23.0 KJ/m |
| -30℃ | ISO 180/1A | 10.00 KJ/m | |
| Shore hardness | ISO 2039-1 | 100.0 Mpa | |
| Tensile modulus | 23℃ | ISO 527-1 | 2400 Mpa |
| Tensile strain | 23℃,Yield | ISO 527-1 | 3.1 % |
| Tensile stress | 23℃,Yield | ISO 527-1 | 46.0 Mpa |
| Electrical performance | Test Condition | Test Method | INEOS STYRO THAILAND/Novodur Ultra 4000PG |
|---|---|---|---|
| Dielectric loss | 23℃,1E+6Hz | IEC 60250 | 0.00870 |
| 23℃,100Hz | IEC 60250 | 0.00630 | |
| Dielectric strength | 23℃,1.00mm | IEC 60243-1 | 38 KV/mm |
| Relative permittivity | 23℃,100Hz | IEC 60250 | 3.00 |
| 23℃,1E+6Hz | IEC 60250 | 2.90 | |
| Surface resistivity | IEC 60093 | 1E+16 ohms | |
| Volume resistivity | IEC 60093 | 1E+16 ohm.cm |
| Physical properties | Test Condition | Test Method | INEOS STYRO THAILAND/Novodur Ultra 4000PG |
|---|---|---|---|
| Shrinkage rate | Across Flow,3.00mm | ISO 294-4 | 0.50-0.80 % |
| Flow,3.00mm | ISO 294-4 | 0.50-0.80 % |