Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

AES W250 TECHNO JAPAN
--
Automotive External Parts
Ultra high impact resista
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | TECHNO JAPAN/W250 |
---|---|---|---|
Rockwell hardness | R-Sale | ISO 2039-2 | 107 |
R-Scale | ASTM D785 | 107 |
thermal performance | Test Condition | Test Method | TECHNO JAPAN/W250 |
---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 92.0 °C |
0.45MPa,Unannealed | ASTM D648 | 105 °C |
mechanical properties | Test Condition | Test Method | TECHNO JAPAN/W250 |
---|---|---|---|
Bending modulus | -- | ISO 178 | 2350 Mpa |
-- | ASTM D790 | 2600 Mpa | |
bending strength | -- | ASTM D790 | 86.3 Mpa |
-- | ISO 178 | 76.0 Mpa | |
tensile strength | Yield | ASTM D638 | 52.0 Mpa |
Yield | ISO 527-2 | 49.0 Mpa |
Physical properties | Test Condition | Test Method | TECHNO JAPAN/W250 |
---|---|---|---|
melt mass-flow rate | 220°C/10.0kg | ISO 1133 | 26 g/10min |
Shrinkage rate | ISO 294-4 | 0.40-0.70 % |