PC/ABS NH-1150HH Samsung Cheil South Korea
INFINO®
Automotive External Parts,Car dashboard
Impact resistance,heat-resisting
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | Samsung Cheil South Korea/NH-1150HH |
|---|---|---|---|
| Rockwell hardness | R-Scale | ASTM D785 | 110 |
| R-Scale | ISO 2039-2 | 110 |
| thermal performance | Test Condition | Test Method | Samsung Cheil South Korea/NH-1150HH |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed,4.00mm | ISO 75-2/A | 81.0 °C |
| 1.8MPa,Unannealed,6.40mm | ASTM D648 | 81.0 °C | |
| 0.45MPa,Unannealed,4.00mm | ISO 75-2/B | 85.0 °C | |
| 0.45MPa,Unannealed,6.40mm | ASTM D648 | 85.0 °C | |
| Vicat softening temperature | ISO 306/B50 | 94.0 °C |
| mechanical properties | Test Condition | Test Method | Samsung Cheil South Korea/NH-1150HH |
|---|---|---|---|
| Bending modulus | ISO 178 | 3600 Mpa | |
| ASTM D790 | 3500 Mpa | ||
| bending strength | ISO 178 | 90.0 Mpa | |
| ASTM D790 | 88.0 Mpa | ||
| elongation | Break | ASTM D638 | 6.0 % |
| Tensile modulus | ASTM D638 | 3000 Mpa | |
| ISO 527-2/50 | 3100 Mpa | ||
| Tensile strain | Break | ISO 527-2/50 | 6.0 % |
| tensile strength | Yield | ASTM D638 | 59.0 Mpa |
| Break | ASTM D638 | 59.0 Mpa | |
| Yield | ISO 527-2/50 | 60.0 Mpa | |
| Break | ISO 527-2/50 | 60.0 Mpa |
| Physical properties | Test Condition | Test Method | Samsung Cheil South Korea/NH-1150HH |
|---|---|---|---|
| melt mass-flow rate | 220°C/10.0kg | ASTM D1238 | 35 g/10min |
| 220°C/10.0kg | ISO 1133 | 35 g/10min | |
| Shrinkage rate | MD:3.20mm | ISO 2577 | 0.20-0.40 % |
| TD:3.20mm | ASTM D955 | 0.20-0.40 % | |
| TD:3.20mm | ISO 2577 | 0.20-0.40 % | |
| MD:3.20mm | ASTM D955 | 0.20-0.40 % |
| impact performance | Test Condition | Test Method | Samsung Cheil South Korea/NH-1150HH |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 7.0 kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 8.0 kJ/m² |
| flammability | Test Condition | Test Method | Samsung Cheil South Korea/NH-1150HH |
|---|---|---|---|
| UL flame retardant rating | 1.0mm | UL 94 | V-1 |
| 1.2mm | UL 94 | V-0 |