Test ConditionTest MethodBada AG/ ASA/PA 320 TM-Z2
Melt volume flow rate220°C/10.0kgISO 113330.0 cm³/10min
Dissipation Factor1MHzIEC 602500.015
Charpy Notched Impact Strength23°CISO 179/1eA14 kJ/m²
Volume resistivityIEC 600931E+13 ohms·cm
relative permittivity1MHzIEC 602502.90
vicatISO 306/B50140 °C
Tensile strain屈服,23°CISO 527-2/503.8 %
density23°CISO 11831.07 g/cm³
Impact strength of simply supported beam without notch23°CISO 179/1eU无断裂
Heat distortion temperature0.45MPa,未退火,HDTISO 75-2/B115 °C
Tensile modulus23°CISO 527-2/11900 MPa
Water absorption rate饱和,23°CISO 626.1 %
tensile strength 屈服,23°CISO 527-2/5045.0 MPa
Water absorption rate平衡,23°C,50%RHISO 621.8 %