Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPS+PPE NORYL GTX™ APS430 resin SABIC
--
--
Filler, glass fiber reinforced material, 30%, filler by weight,
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | SABIC/NORYL GTX™ APS430 resin |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed,6.40mm | ASTM D648 | 255 °C |
| 0.45MPa,Unannealed,3.20mm | ASTM D648 | 255 °C | |
| Linear coefficient of thermal expansion | MD:-30to30°C | ASTME831 | 1.8E-5到5.8E-5 cm/cm/°C |
| mechanical properties | Test Condition | Test Method | SABIC/NORYL GTX™ APS430 resin |
|---|---|---|---|
| Bending modulus | ASTM D790 | 8620 MPa | |
| bending strength | ASTM D790 | 167 MPa | |
| elongation | Break | Internal Method | 10 % |
| tensile strength | Yield | Internal Method | 123 MPa |
| Electrical performance | Test Condition | Test Method | SABIC/NORYL GTX™ APS430 resin |
|---|---|---|---|
| Dielectric constant | 50Hz | ASTM D150 | 3.30 |
| 60Hz | ASTM D150 | 3.30 | |
| Surface resistivity | ASTM D257 | 1E+16 ohms |
| Physical properties | Test Condition | Test Method | SABIC/NORYL GTX™ APS430 resin |
|---|---|---|---|
| density | ASTM D792 | 1.48 g/cm³ | |
| melt mass-flow rate | 300°C/5.0kg | ASTM D1238 | 44 g/10min |
| Shrinkage rate | MD:3.20mm | Internal Method | 0.30to0.70 % |
| Water absorption rate | 24hr | ASTM D570 | 0.020 % |
| impact performance | Test Condition | Test Method | SABIC/NORYL GTX™ APS430 resin |
|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 78 J/m |
| flammability | Test Condition | Test Method | SABIC/NORYL GTX™ APS430 resin |
|---|---|---|---|
| UL flame retardant rating | 0.800mm | UL 94 | V-0 |
| 0.8mm | UL 94 | V-0 |