| elastomer | Test Condition | Test Method | HUNTSMAN GERMANY/A 98 P 4772 |
|---|---|---|---|
| tensile strength | Break | ASTM D-412 | 44.8 Mpa |
| 100%Strain | ASTM D-412 | 16.5 Mpa | |
| Permanent compression deformation | 23°C, 24.0 hr | ASTM D395 | 32 % |
| elongation | Break | ASTM D-412 | 400 % |
| tear strength | ASTM D-624 | 135 kN/m | |
| Physical properties | Test Condition | Test Method | HUNTSMAN GERMANY/A 98 P 4772 |
| Shrinkage rate | MD | Internal Method | 0.30 % |
| thermal performance | Test Condition | Test Method | HUNTSMAN GERMANY/A 98 P 4772 |
| Melting temperature | Internal Method | 145 to 200 °C | |
| hardness | Test Condition | Test Method | HUNTSMAN GERMANY/A 98 P 4772 |
| Shore hardness | ASTM D-2240 | 52 | |
| mechanical properties | Test Condition | Test Method | HUNTSMAN GERMANY/A 98 P 4772 |
| Wear resistance | DIN 53516 | 30 mm³ |