Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PA66 66 MV HI LYONDELLBASELL GERMANY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodLYONDELLBASELL GERMANY/66 MV HI
Impact strength of simply supported beam without notch23°C无断裂
-30°C无断裂
hardnessTest ConditionTest MethodLYONDELLBASELL GERMANY/66 MV HI
ball-indentation hardnessISO 2039-1110 Mpa
Mechanical propertiesTest ConditionTest MethodLYONDELLBASELL GERMANY/66 MV HI
Tensile strain (yield)ISO 527-2/1A/505 %
Tensile modulusISO 527-1/1A/12500 Mpa
Tensile stress (yield)ISO 527-2/1A/5065 Mpa
Electrical performanceTest ConditionTest MethodLYONDELLBASELL GERMANY/66 MV HI
Compared to the Leakage Tracking Index (CTI)IEC 60112PLC 0
Volume resistivityIEC 62631-3-1> 1.0E+13 ohms·m
Surface ResistivityIEC 60093> 1.0E+15 ohms
flammabilityTest ConditionTest MethodLYONDELLBASELL GERMANY/66 MV HI
Flammability level3.0 mmHB
burning rate2.00 mmISO 379530 mm/min
2.00 mmFMVSS 30230 mm/min
Burning wire flammability index3.0 mm600 °C
1.5 mm600 °C
Flammability level1.5 mmHB
0.75 mmHB
physical property Test ConditionTest MethodLYONDELLBASELL GERMANY/66 MV HI
Water absorption rate平衡, 23°C, 50% RHISO 622.1 %
Thermal performanceTest ConditionTest MethodLYONDELLBASELL GERMANY/66 MV HI
Heat distortion temperature0.45 MPa, 未退火,HDTISO 75-2/Bf170 °C
1.8 MPa, 未退火,HDTISO 75-2/Af60 °C
vicat--ISO 306/A50230 °C
--ISO 306/B50215 °C
ball-indentation hardness(60°C)IEC 60695-10-2通过
injectionTest ConditionTest MethodLYONDELLBASELL GERMANY/66 MV HI
Suggested maximum moisture content0.040 to 0.10
Processing (melt) temperature270 to 290
drying temperature80
Temperature60 to 100
drying time3.0 to 4.0