Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC/PBT TV4 660SN DSM HOLAND
Arnite®
--
Filler: Glass fiber reinf,30% filler by weight
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | DSM HOLAND/TV4 660SN |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 180 °C |
| Melting temperature | ISO 11357-3 | 225 °C |
| mechanical properties | Test Condition | Test Method | DSM HOLAND/TV4 660SN |
|---|---|---|---|
| Tensile modulus | ISO 527-2 | 10500 Mpa | |
| Tensile strain | Break | ISO 527-2 | 2.0 % |
| tensile strength | Break | ISO 527-2 | 130 Mpa |
| impact performance | Test Condition | Test Method | DSM HOLAND/TV4 660SN |
|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 55 kJ/m² |
| flammability | Test Condition | Test Method | DSM HOLAND/TV4 660SN |
|---|---|---|---|
| Flammability level | 1.5mm | IEC 60695-11-10,-20 | V-0 |
| 0.75mm | IEC 60695-11-10,-20 | V-0 |