Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPO APS130-7002 SABIC INNOVATIVE US
NORYL GTX™
medical care
Thermal stability,Glass fiber reinforced,Filler: Glass fiber reinf,30% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/APS130-7002 |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed,3.20mm | ASTM D648 | 267 °C |
0.45MPa,Unannealed,6.40mm | ASTM D648 | 267 °C | |
Linear coefficient of thermal expansion | MD:-30to30°C | ASTME831 | 2.5E-5到5.5E-5 cm/cm/°C |
mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/APS130-7002 |
---|---|---|---|
Bending modulus | ASTM D790 | 8430 Mpa | |
bending strength | ASTM D790 | 157 Mpa | |
elongation | Break | Internal Method | 8.0 % |
tensile strength | Yield | Internal Method | 113 Mpa |
Electrical performance | Test Condition | Test Method | SABIC INNOVATIVE US/APS130-7002 |
---|---|---|---|
Dielectric constant | 50Hz | ASTM D150 | 3.30 |
60Hz | ASTM D150 | 3.30 | |
Dielectric strength | 1.60mm,inOil | ASTM D149 | 22 KV/mm |
Surface resistivity | ASTM D257 | 1E+16 ohms |
Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/APS130-7002 |
---|---|---|---|
melt mass-flow rate | 300°C/5.0kg | ASTM D1238 | 29 g/10min |
Shrinkage rate | MD:3.20mm | Internal Method | 0.25-0.70 % |
Water absorption rate | 24hr | ASTM D570 | 0.020 % |