Phenolic SumiDurez 115 SumiDurez Singapore Pte Ltd
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | SumiDurez Singapore Pte Ltd/SumiDurez 115 |
---|---|---|---|
Impact strength of cantilever beam gap | 模压成型 | ASTM D256 | 16 J/m |
Mechanical properties | Test Condition | Test Method | SumiDurez Singapore Pte Ltd/SumiDurez 115 |
---|---|---|---|
compressive strength | ASTM D695 | 221 MPa | |
Tensile modulus | 模压成型 | ASTM D638 | 9650 MPa |
bending strength | 模压成型 | ASTM D790 | 72.4 MPa |
tensile strength | 屈服,模压成型 | ASTM D638 | 55.2 MPa |
Electrical performance | Test Condition | Test Method | SumiDurez Singapore Pte Ltd/SumiDurez 115 |
---|---|---|---|
Volume resistivity | ASTM D257 | 1E+12 ohms·cm | |
dielectric strength | ASTM D149 | 13 kV/mm |
flammability | Test Condition | Test Method | SumiDurez Singapore Pte Ltd/SumiDurez 115 |
---|---|---|---|
UL flame retardant rating | 3.2mm | UL 94 | V-0 |
physical property | Test Condition | Test Method | SumiDurez Singapore Pte Ltd/SumiDurez 115 |
---|---|---|---|
Shrinkage rate | ASTM D1895 | 2.5 | |
MD:模压成型 | ASTM D955 | 0.60to1.1 % | |
Water absorption rate | 24hr | ASTM D570 | 0.40 % |
Apparent density | ASTM D1895 | 0.56 g/cm³ | |
density | ASTM D792 | 1.40 g/cm³ |
Thermal performance | Test Condition | Test Method | SumiDurez Singapore Pte Ltd/SumiDurez 115 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,模压成型,HDT | ASTM D648 | 191 °C |