Copolyester Eastar™ MN210, Natural Eastman Chemical Company
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodEastman Chemical Company/Eastar™ MN210, Natural
Impact strength of cantilever beam gap-40°CASTM D25637 J/m
Suspended wall beam without notch impact strength-40°CASTM D4218无断裂
Impact strength of cantilever beam gap23°CASTM D256100 J/m
Suspended wall beam without notch impact strength23°CASTM D4218无断裂
hardnessTest ConditionTest MethodEastman Chemical Company/Eastar™ MN210, Natural
Rockwell hardnessR级,23°CASTM D785106
Mechanical propertiesTest ConditionTest MethodEastman Chemical Company/Eastar™ MN210, Natural
bending strength23°CASTM D79070.0 MPa
tensile strength 断裂,23°CASTM D63828.0 MPa
Flexural modulus23°CASTM D7902100 MPa
elongation屈服,23°CASTM D6384.0 %
tensile strength 屈服,23°CASTM D63850.0 MPa
elongation断裂,23°CASTM D638110 %
physical property Test ConditionTest MethodEastman Chemical Company/Eastar™ MN210, Natural
Shrinkage rateMD:3.20mmASTM D9550.20to0.50 %
Water absorption rate23°C,24hrASTM D5700.13 %
densityASTM D7921.27 g/cm³
Thermal performanceTest ConditionTest MethodEastman Chemical Company/Eastar™ MN210, Natural
Heat distortion temperature1.8MPa,未退火,HDTASTM D64863.0 °C
vicatASTM D152585.0 °C
Heat distortion temperature0.45MPa,未退火,HDTASTM D64870.0 °C
thermal conductivity23°C0.19 W/m/K