Material Comparison
Add Comparison Model
Highlight Differences
Hide Same

Product Name / Manufacturer / Model

Brand

Typical Applications

Properties

Color

Form

Processing Methods

Grade

Filler

Recycled Content

Certificates

Reference Price

hardnessTest ConditionTest MethodDUPONT USA/73G30HSL BK416
Ball Pressure TestH961/30ISO 2039-1230 Mpa
Rockwell hardnessR-ScaleISO 2039-2121
mechanical propertiesTest ConditionTest MethodDUPONT USA/73G30HSL BK416
bending strengthISO 178280 Mpa
Tensile creep modulus1hrISO 899-1-- Mpa
Tensile strainBreakISO 527-23.5 %
tensile strengthBreakISO 527-2190 Mpa
Tensile modulusISO 527-29500 Mpa
Bending modulusISO 1788500 Mpa
Tensile creep modulus1000hrISO 899-1-- Mpa
Supplementary InformationTest ConditionTest MethodDUPONT USA/73G30HSL BK416
EmissionofOrganicCompoundsVDA2778.50 µgC/g
OdorVDA2703.50
flammabilityTest ConditionTest MethodDUPONT USA/73G30HSL BK416
UL flame retardant rating1.5mmIEC 60695-11-10,-20HB
0.75mmUL 94HB
Extreme Oxygen IndexISO 4589-221 %
Burning rate1.00mmISO 379550 mm/min
AtomizationG-value(condensate)ISO 64521E-04 g
F-value(refraction)ISO 645295 %
UL flame retardant rating1.5mmUL 94HB
FMVSS flammabilityFMVSS302B
UL flame retardant rating0.75mmIEC 60695-11-10,-20HB
impact performanceTest ConditionTest MethodDUPONT USA/73G30HSL BK416
Multi axis Instrumented Impact Energy23°CISO 6603-23.50 J
Charpy Notched Impact Strength-30°CISO 179/1eA10 kJ/m²
Impact strength of cantilever beam gap23°CISO 180/1A15 kJ/m²
Impact strength of simply supported beam without notch23°CISO 179/1eU100 kJ/m²
-30°CISO 179/1eU80 kJ/m²
Charpy Notched Impact Strength23°CISO 179/1eA16 kJ/m²
Impact strength of cantilever beam gap-30°CISO 180/1A10 kJ/m²
Suspended wall beam without notch impact strength23°CISO 180/1U80 kJ/m²
Physical propertiesTest ConditionTest MethodDUPONT USA/73G30HSL BK416
densityISO 11831.36 g/cm³
MediumDensity1.20 g/cm³
Shrinkage rateMDISO 294-40.20 %
Melt Volume Flow Rate (MVR)250°C/5.0kgISO 113315.0 cm3/10min
Water absorption rateSaturation,23°C,2.00mmISO 626.3 %
Equilibrium,23°C,2.00mm,50%RHISO 621.9 %
ThermalConductivityofMelt0.26 W/m/K
SpecificHeatCapacity of Melt2280 J/kg/°C
Shrinkage rateTDISO 294-40.60 %
thermal performanceTest ConditionTest MethodDUPONT USA/73G30HSL BK416
Effective thermal diffusivity coefficient9.1E-08 m²/s
Linear coefficient of thermal expansionMDISO 11359-22.6E-05 cm/cm/°C
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B220 °C
Glass transition temperatureISO 11357-260.0 °C
Linear coefficient of thermal expansionTDISO 11359-27.5E-05 cm/cm/°C
Hot deformation temperature1.8MPa,UnannealedISO 75-2/A210 °C
Melting temperatureISO 11357-3221 °C
Vicat softening temperatureISO 306/B50215 °C