Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PET TAROLOX 111 G4 Taro Plast S.p.A.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodTaro Plast S.p.A./TAROLOX 111 G4
Charpy Notched Impact Strength23°CISO 1798.0 kJ/m²
Impact strength of cantilever beam gap23°C,3.20mmASTMD25670 J/m
Impact strength of simply supported beam without notch23°CISO 17942 kJ/m²
Electrical performanceTest ConditionTest MethodTaro Plast S.p.A./TAROLOX 111 G4
dielectric strength1.00mmASTM D14934 kV/mm
Compared to the Leakage Tracking Index (CTI)解决方案AIEC 60112PLC 2
Mechanical propertiesTest ConditionTest MethodTaro Plast S.p.A./TAROLOX 111 G4
Flexural modulusASTMD7907800 MPa
elongation断裂ASTMD6382.8 %
bending strength断裂ASTM D790170 MPa
Tensile modulusASTMD6388200 MPa
tensile strength 断裂ASTMD638120 MPa
bending strength--ISO 178170 MPa
flammabilityTest ConditionTest MethodTaro Plast S.p.A./TAROLOX 111 G4
Hot filament ignition temperature2.0mmIEC 60695-2-13750 °C
UL flame retardant rating1.0mmUL 94HB
Limiting Oxygen IndexASTM D286324 %
physical property Test ConditionTest MethodTaro Plast S.p.A./TAROLOX 111 G4
Shrinkage rateMDASTM D9550.30to0.50 %
GranuleHumidity内部方法<0.050 %
Water absorption rate23°C,24hrASTMD5700.060 %
densityASTMD7921.48to1.50 g/cm³
Shrinkage rateTDASTM D9550.40to0.70 %
Thermal performanceTest ConditionTest MethodTaro Plast S.p.A./TAROLOX 111 G4
Heat distortion temperature1.8MPa,未退火,HDTASTMD648230 °C
Linear coefficient of thermal expansionMD:-30到30°CASTM D6963.5E-05 cm/cm/°C
ball-indentation hardness245°CVDE0470通过
vicatISO 306/B50226 °C
melting temperatureASTMD211252 °C