ASA WR-9300HF Samsung Cheil South Korea
STAREX® 
Electronic and electrical、Automotive components
UV resistance、High temperature resistan
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodSamsung Cheil South Korea/WR-9300HF
Charpy Notched Impact Strength23°CISO 179/1eA13 kJ/m²
Impact strength of cantilever beam gap-30°CISO 180/1A5.5 kJ/m²
23°CISO 180/1A12 kJ/m²
hardnessTest ConditionTest MethodSamsung Cheil South Korea/WR-9300HF
Rockwell hardnessR级ISO 2039-2106
R级ASTM D785106
Mechanical propertiesTest ConditionTest MethodSamsung Cheil South Korea/WR-9300HF
tensile strength 屈服ISO 527-2/544.0 Mpa
elongation断裂ASTM D63815 %
bending strengthISO 17867.0 Mpa
Flexural modulusISO 1782100 Mpa
bending strengthASTM D79066.7 Mpa
tensile strength 屈服ASTM D63844.1 Mpa
Flexural modulusASTM D7902160 Mpa
optical performance Test ConditionTest MethodSamsung Cheil South Korea/WR-9300HF
Yellowness Index3.20mmASTM D192525 YI
flammabilityTest ConditionTest MethodSamsung Cheil South Korea/WR-9300HF
UL flame retardant rating1.5mmUL 94HB
physical property Test ConditionTest MethodSamsung Cheil South Korea/WR-9300HF
melt mass-flow rate250°C/2.16kgASTM D12386.5 g/10min
250°C/2.16kgISO 11336.5 g/10min
Shrinkage rateMD:3.20mmASTM D9550.40-0.70 %
TD:3.20mmISO 25770.40-0.70 %
TD:3.20mmASTM D9550.40-0.70 %
melt mass-flow rate220°C/10.0kgASTM D123812 g/10min
220°C/10.0kgISO 113312 g/10min
Shrinkage rateMD:3.20mmISO 25770.40-0.70 %
Thermal performanceTest ConditionTest MethodSamsung Cheil South Korea/WR-9300HF
Heat distortion temperature1.8MPa,Unannealed,4.00mm,HDTISO 75-2/A80.0 °C
1.8MPa,未退火,6.40mm,HDTASTM D64887.0 °C
vicatISO 306/B50100 °C
Heat distortion temperature0.45MPa,未退火,3.20mm,HDTASTM D64886.0 °C
0.45MPa,未退火,6.40mm,HDTASTM D64892.0 °C
1.8MPa,未退火,3.20mm,HDTASTM D64873.0 °C

Contact Us