Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP Homopolymer HIPOLEN P® TA 41 Hipol a.d.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | Hipol a.d./HIPOLEN P® TA 41 |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 85.0 °C |
| Vicat softening temperature | ISO 306/A50 | 140 °C |
| mechanical properties | Test Condition | Test Method | Hipol a.d./HIPOLEN P® TA 41 |
|---|---|---|---|
| Bending modulus | ASTM D790 | 1300 MPa | |
| elongation | Yield | ASTM D638 | 8.0 % |
| Break | ASTM D638 | 800 % | |
| tensile strength | Yield | ASTM D638 | 30.0 MPa |
| Physical properties | Test Condition | Test Method | Hipol a.d./HIPOLEN P® TA 41 |
|---|---|---|---|
| density | ASTM D1505 | 0.910 g/cm³ | |
| melt mass-flow rate | 230°C/2.16kg | ASTM D1238 | 8.0 g/10min |
| impact performance | Test Condition | Test Method | Hipol a.d./HIPOLEN P® TA 41 |
|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ASTM D256 | 35 J/m |