| impact performance | Test Condition | Test Method | BOREALIS EUROPE/BHC5012C |
|---|---|---|---|
| Charpy Notched Impact Strength | -20°C,Injection | ISO 179/1eA | 4.5 kJ/m² |
| -30°C,Injection | ISO 179/1eA | 3.8 kJ/m² | |
| Impact strength of simply supported beam without notch | 23°C,Injection | ISO 179/1eU | NoBreak |
| Charpy Notched Impact Strength | 23°C,Injection | ISO 179/1eA | 75 kJ/m² |
| Impact strength of cantilever beam gap | -20°C,Injection | ISO 180/1A | 5.5 kJ/m² |
| Impact strength of simply supported beam without notch | -20°C,Injection | ISO 179/1eU | NoBreak |
| Impact strength of cantilever beam gap | 23°C,Injection | ISO 180/1A | 55 kJ/m² |
| Physical properties | Test Condition | Test Method | BOREALIS EUROPE/BHC5012C |
| density | ISO 1183 | 0.905 g/cm³ | |
| Shrinkage rate | MD | Internal Method | 1.9 % |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 0.30 g/10min |
| mechanical properties | Test Condition | Test Method | BOREALIS EUROPE/BHC5012C |
| tensile strength | Yield,Injection | ISO 527-2/50 | 27.0 Mpa |
| Tensile modulus | Injection | ISO 527-2/1 | 1150 Mpa |
| Bending modulus | Injection | ISO 178 | 1350 Mpa |
| bending strength | Injection | ISO 178 | 35.0 Mpa |
| Tensile strain | Yield,Injection | ISO 527-2/50 | 11 % |
| thermal performance | Test Condition | Test Method | BOREALIS EUROPE/BHC5012C |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 80.0 °C |
| MeltEnergy | ISO 11357 | 86.8 kJ/kg | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 50.0 °C |
| Vicat softening temperature | ISO 306/B50 | 65.0 °C |