PA9T TA112 KURARAY JAPAN
Genestar™
--
heat-resisting
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | KURARAY JAPAN/TA112 |
|---|---|---|---|
| Hot deformation temperature | 1.8 MPa, Unannealed | ASTM D648 | 275 °C |
| mechanical properties | Test Condition | Test Method | KURARAY JAPAN/TA112 |
|---|---|---|---|
| Bending modulus | ASTM D790 | 6000 Mpa | |
| bending strength | ASTM D790 | 140 Mpa | |
| elongation | Break | ASTM D638 | 1.5 % |
| tensile strength | ASTM D638 | 75.0 Mpa |
| Electrical performance | Test Condition | Test Method | KURARAY JAPAN/TA112 |
|---|---|---|---|
| Volume resistivity | ASTM D257 | 1.0E+16 ohms·cm |
| Physical properties | Test Condition | Test Method | KURARAY JAPAN/TA112 |
|---|---|---|---|
| Shrinkage rate | Across FlowFlow : 1.00 mm | 0.90 % | |
| Flow : 1.00 mm | 0.50 % |
| flammability | Test Condition | Test Method | KURARAY JAPAN/TA112 |
|---|---|---|---|
| Bar Flow Length | 320°C, 500.0 μm | 4.40 CM | |
| UL flame retardant rating | 3.0 mm | UL 94 | HB |