| mechanical properties | Test Condition | Test Method | LUBRIZOL USA/X585A-4 |
|---|---|---|---|
| tensile strength | Yield | MPa | |
| elongation | Break | 650 % | |
| tensile strength | 300%Strain | MPa | |
| tear strength | ASTM D-624 | 108 kN/m | |
| tensile strength | 100%Strain | ASTM D-412 | 6.86 Mpa |
| Permanent compression deformation | 23℃,22.0hr | ASTM D-395 | 15 % |
| Physical properties | Test Condition | Test Method | LUBRIZOL USA/X585A-4 |
| Shore hardness | ShoreA | ASTM D-2240 | 87 |
| melt mass-flow rate | 190℃/8.7kg | ASTM D-1238 | 15 g/10min |
| Thermal properties | Test Condition | Test Method | LUBRIZOL USA/X585A-4 |
| Vicat softening temperature | ASTM D-1525 | 95 °C |