PA66 NYLOY® MG-0033N NYTEX COMPOSITES
--
--
Filler, glass fiber reinforced material, 33%, filler by weight,
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | NYTEX COMPOSITES/NYLOY® MG-0033N |
|---|---|---|---|
| Rockwell hardness | R-Sale | ISO 2039-2 | 115 |
| R-Scale | ASTM D785 | 115 |
| thermal performance | Test Condition | Test Method | NYTEX COMPOSITES/NYLOY® MG-0033N |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 250 °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 245 °C |
| mechanical properties | Test Condition | Test Method | NYTEX COMPOSITES/NYLOY® MG-0033N |
|---|---|---|---|
| Bending modulus | -- | ISO 178 | 8700 MPa |
| -- | ASTM D790 | 10000 MPa | |
| bending strength | -- | ASTM D790 | 265 MPa |
| -- | ISO 178 | 270 MPa | |
| elongation | Break | ISO 527-2 | 3.2 % |
| Break | ASTM D638 | 2.0 % | |
| tensile strength | -- | ASTM D638 | 177 MPa |
| -- | ISO 527-2 | 180 MPa |
| Physical properties | Test Condition | Test Method | NYTEX COMPOSITES/NYLOY® MG-0033N |
|---|---|---|---|
| density | -- | ISO 1183 | 1.38 g/cm³ |
| -- | ASTM D792 | 1.18 g/cm³ | |
| Shrinkage rate | MD | ISO 294-4 | 0.43 % |
| MD | ASTM D955 | 0.43 % | |
| TD | ISO 294-4 | 1.2 % | |
| TD | ASTM D955 | 1.2 % |
| impact performance | Test Condition | Test Method | NYTEX COMPOSITES/NYLOY® MG-0033N |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 15 kJ/m² |
| Impact strength of cantilever beam gap | 23°C,3.18mm | ASTM D256 | 160 J/m |