Plastic Datasheets

Impact resistanceTest ConditionTest MethodPolymer Resources Ltd./PRL PC-GP1-TFE10
Dart impact3.18mmASTM D302936.2 J
Impact strength of cantilever beam gap23°C,3.18mmASTM D256160 J/m
Mechanical propertiesTest ConditionTest MethodPolymer Resources Ltd./PRL PC-GP1-TFE10
Flexural modulus3.17mmASTM D7902070 MPa
tensile strength 屈服,3.17mmASTM D63855.2 MPa
Break,3.18mmASTM D63855.2 MPa
bending strength3.18mmASTM D79082.7 MPa
physical property Test ConditionTest MethodPolymer Resources Ltd./PRL PC-GP1-TFE10
densityASTM D7921.22 g/cm³
Shrinkage rateMD:3.18mmASTM D9550.50to0.70 %
melt mass-flow rate300°C/1.2kgASTM D12387.0to12 g/10min
Thermal performanceTest ConditionTest MethodPolymer Resources Ltd./PRL PC-GP1-TFE10
Heat distortion temperature0.45MPa,未退火,3.18mm,HDTASTM D648137 °C
1.8MPa,未退火,3.18mm,HDTASTM D648131 °C