Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Certificates
Reference Price
| thermal performance | Test Condition | Test Method | EXXONMOBIL USA/AP3AW |
|---|---|---|---|
| Hot deformation temperature | 455KPa | ASTM D-648 | 104 °C |
| Typical processing temperature | 200-250 °C | ||
| mechanical properties | Test Condition | Test Method | EXXONMOBIL USA/AP3AW |
| Gardner impact strength | 3.2mmt,-29℃ | ASTM D-5420 | 20 J |
| Bending modulus | 1.3mm/min | ASTM D-790A | 1317 Mpa |
| Impact strength of cantilever beam gap | 23℃ | ASTM D-256 | 86 J/m |
| Elongation at Break | 2in/min,50mm/min | ASTM D-638 | 7 % |
| tensile strength | 2in/min,50mm/min,Yield | ASTM D-638 | 27 Mpa |
| Basic Performance | Test Condition | Test Method | EXXONMOBIL USA/AP3AW |
| density | ASTM D-792 | 0.9 g/cm³ | |
| melt mass-flow rate | 230℃,2.16kg | ASTM D-1238 | 10 g/10min |