Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

Rubber Techsil® RTV27844 Techsil Limited
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
optical performance | Test Condition | Test Method | Techsil Limited/Techsil® RTV27844 |
---|---|---|---|
refractive index | 1.406 |
Uncured Properties | Test Condition | Test Method | Techsil Limited/Techsil® RTV27844 |
---|---|---|---|
MixRatiobyWeight(PBW) | PartB | 1.0 | |
Curing Time | 150°C | 15 hr | |
MixRatiobyWeight(PBW) | 粘度 | 4.0 Pa·s | |
密度 | 1.02 g/cm³ | ||
Curing Time | 125°C | 0.75 hr | |
100°C | 1.0 hr | ||
25°C | 1.4E+2到1.7E+2 hr | ||
储存稳定性(25°C) | 240 min | ||
MixRatiobyWeight(PBW) | PartA | 10 | |
Curing Time | 65°C | 4.0 hr |
Cured Properties | Test Condition | Test Method | Techsil Limited/Techsil® RTV27844 |
---|---|---|---|
Dissipation Factor | 1kHz | 6E-04 | |
Volume resistivity | 1.8E+15 ohms·cm | ||
Shore hardness | ShoreA | 44 | |
relative permittivity | 1kHz | 2.70 | |
dielectric strength | 1.90mm | 20 kV/mm | |
tensile strength | 6.37 MPa | ||
elongation | 断裂 | 120 % |
physical property | Test Condition | Test Method | Techsil Limited/Techsil® RTV27844 |
---|---|---|---|
Shrinkage rate | MD | 0.20 % |
Thermal performance | Test Condition | Test Method | Techsil Limited/Techsil® RTV27844 |
---|---|---|---|
thermal conductivity | 0.19 W/m/K | ||
Usage temperature | -60-240 °C | ||
Linear coefficient of thermal expansion | MD | 2.7E-04 cm/cm/°C | |
specific heat | 1260 J/kg/°C |
Contact Us
Get App
Top