Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP B393G SK KOREA
YUPLENE®
Electrical field,Automotive sector,Electronic field,container,Thin walled components,Industrial applications
Impact copolymer,Dimensional stability,High rigidity,High impact resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | SK KOREA/B393G |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ASTM D256 | 69 J/m |
-20°C | ASTM D256 | 49 J/m |
hardness | Test Condition | Test Method | SK KOREA/B393G |
---|---|---|---|
Rockwell hardness | R级 | ASTM D785 | 90 |
Supplementary Information | Test Condition | Test Method | SK KOREA/B393G |
---|---|---|---|
DuPontImpactStrength | -10°C | ASTM D2794 | >1.96 J |
Mechanical properties | Test Condition | Test Method | SK KOREA/B393G |
---|---|---|---|
elongation | 断裂 | ASTM D638 | <500 % |
tensile strength | 屈服 | ASTM D638 | 26.5 Mpa |
Flexural modulus | ASTM D790 | 1370 Mpa |
physical property | Test Condition | Test Method | SK KOREA/B393G |
---|---|---|---|
spiral flow length | 内部方法 | >80.0 CM | |
melt mass-flow rate | 230°C/2.16kg | ASTM D1238 | 60 g/10min |
aging | Test Condition | Test Method | SK KOREA/B393G |
---|---|---|---|
Accelerated oven aging in the air | 150°C | ASTM D3012 | 15.0 day |
Thermal performance | Test Condition | Test Method | SK KOREA/B393G |
---|---|---|---|
vicat | ASTM D1525 | 150 °C | |
Heat distortion temperature | HDT | ASTM D648 | 110 °C |