Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP AW864 TPC SINGAPORE
COSMOPLENE®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Supplementary Information | Test Condition | Test Method | TPC SINGAPORE/AW864 |
|---|---|---|---|
| WeatherResistance | 63°C | Internal Method | 1.4 month |
| hardness | Test Condition | Test Method | TPC SINGAPORE/AW864 |
|---|---|---|---|
| Rockwell hardness | R-Scale | ASTM D785 | 91 |
| thermal performance | Test Condition | Test Method | TPC SINGAPORE/AW864 |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 124 °C |
| mechanical properties | Test Condition | Test Method | TPC SINGAPORE/AW864 |
|---|---|---|---|
| Bending modulus | ASTM D790 | 1290 Mpa | |
| elongation | Break | ASTM D638 | 300 % |
| tensile strength | Yield | ASTM D638 | 27.5 Mpa |
| Break | ASTM D638 | 23.0 Mpa |
| Electrical performance | Test Condition | Test Method | TPC SINGAPORE/AW864 |
|---|---|---|---|
| Surface resistivity | ASTM D257 | 1E+13 ohms |
| Physical properties | Test Condition | Test Method | TPC SINGAPORE/AW864 |
|---|---|---|---|
| density | ASTM D792 | 0.900 g/cm³ | |
| melt mass-flow rate | ASTM D1238 | 9.0 g/10min | |
| Shrinkage rate | MD:2.00mm | Internal Method | 1.6 % |
| TD:2.00mm | Internal Method | 1.7 % |
| impact performance | Test Condition | Test Method | TPC SINGAPORE/AW864 |
|---|---|---|---|
| Impact strength of cantilever beam gap | -20°C | ASTM D256 | 45 J/m |
| 23°C | ASTM D256 | 92 J/m |
| flammability | Test Condition | Test Method | TPC SINGAPORE/AW864 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |