Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

ABS HH-112 INEOS STYRO THAILAND
Novodur®
Automotive interior parts,Electronic field
heat-resisting,High rigidity
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | INEOS STYRO THAILAND/HH-112 |
|---|---|---|---|
| Hot deformation temperature | 1.8Mpa | ASTM D648 | 109 °C |
| UL flame retardant rating | UL 94 | HB | |
| Vicat softening temperature | ISO 306 | 112 °C |
| mechanical properties | Test Condition | Test Method | INEOS STYRO THAILAND/HH-112 |
|---|---|---|---|
| Bending modulus | ISO 178 | 27000 kg/cm | |
| bending strength | ISO 178 | 880 kg/cm | |
| elongation | Yield | ISO 527-2 | 3.0 % |
| Break | ISO 527-2 | 20 % | |
| Rockwell hardness | 115 R | ||
| Tensile modulus | ISO 527-2 | 28000 kg/cm | |
| tensile strength | Break | ISO 527-2 | 390 kg/cm |
| Yield | ISO 527-2 | 580 kg/cm |
| Physical properties | Test Condition | Test Method | INEOS STYRO THAILAND/HH-112 |
|---|---|---|---|
| Water absorption rate | ASTM D570 | 0.3 % |