Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA12 Grilamid® LV-3 ESD EMS-GRIVORY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | EMS-GRIVORY/Grilamid® LV-3 ESD |
---|---|---|---|
Charpy Notched Impact Strength | -30°C | kJ/m² | 10 10 |
Impact strength of simply supported beam without notch | 23°C | kJ/m² | 85 80 |
Charpy Notched Impact Strength | 23°C | kJ/m² | 15 15 |
Impact strength of simply supported beam without notch | -30°C | kJ/m² | 70 65 |
hardness | Test Condition | Test Method | EMS-GRIVORY/Grilamid® LV-3 ESD |
---|---|---|---|
Shore hardness | 邵氏D,15秒 | 83 81 |
Mechanical properties | Test Condition | Test Method | EMS-GRIVORY/Grilamid® LV-3 ESD |
---|---|---|---|
tensile strength | 断裂 | MPa | 125 110 |
Tensile strain | 断裂 | % | 5.0 7.0 |
Tensile modulus | MPa | 7800 7000 |
Electrical performance | Test Condition | Test Method | EMS-GRIVORY/Grilamid® LV-3 ESD |
---|---|---|---|
Surface Resistivity | ohms | -- 1E+06 | |
Volume resistivity | ohms·cm | 1E+06 1E+06 |
flammability | Test Condition | Test Method | EMS-GRIVORY/Grilamid® LV-3 ESD |
---|---|---|---|
Flammability level | 0.8mm | HB -- |
physical property | Test Condition | Test Method | EMS-GRIVORY/Grilamid® LV-3 ESD |
---|---|---|---|
Shrinkage rate | MD | % | 0.10 -- |
density | g/cm³ | 1.28 -- | |
Water absorption rate | 饱和,23°C | % | 1.1 -- |
Shrinkage rate | TD | % | 0.80 -- |
Water absorption rate | 平衡,23°C,50%RH | % | 0.60 -- |
Thermal performance | Test Condition | Test Method | EMS-GRIVORY/Grilamid® LV-3 ESD |
---|---|---|---|
Continuous use temperature | --2 | °C | 90.0to120 -- |
--3 | °C | 150 -- | |
melting temperature | °C | 178 -- | |
Linear coefficient of thermal expansion | MD | cm/cm/°C | 5E-05 -- |
Heat distortion temperature | 1.8MPa,未退火,HDT | °C | 160 -- |
8.0MPa,未退火,HDT | °C | 90.0 -- | |
Linear coefficient of thermal expansion | TD | cm/cm/°C | 1.2E-04 -- |