Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA/ABS N NG-04 BASF GERMANY
Terblend®
Automotive sector、Shell
dimensional stability 、High rigidity
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | BASF GERMANY/N NG-04 |
---|---|---|---|
Heat Deflection Temperature | 0.45MPa,Annealed | ISO75-2/B | 164 °C |
Linear thermal expansion coefficient | MD | ISO11359-2 | 4E-05 cm/cm/°C |
Vicat Softening Temperature | -- | ISO306/B50 | 114 °C |
Heat Deflection Temperature | 1.8MPa,退火 | ISO75-2/A | 100 °C |
Vicat Softening Temperature | -- | ISO306/A50 | 180 °C |
Hardness | Test Condition | Test Method | BASF GERMANY/N NG-04 |
---|---|---|---|
Ball Indentation Hardness | ISO2039-1 | 107 Mpa |
Films Properties | Test Condition | Test Method | BASF GERMANY/N NG-04 |
---|---|---|---|
Elongation - MD | 断裂 | ISO527-3 | 3.2 % |
Mechanical Properties | Test Condition | Test Method | BASF GERMANY/N NG-04 |
---|---|---|---|
Flexural Modulus | ISO178 | 4500 Mpa | |
Tensile Strain | 屈服,23°C | ISO527-2 | 3.2 % |
Flexural Stress | ISO178 | 115 Mpa | |
Tensile Stress | 屈服,23°C | ISO527-2 | 60.0 Mpa |
Tensile Modulus | ISO527-2 | 5400 Mpa |
Physical | Test Condition | Test Method | BASF GERMANY/N NG-04 |
---|---|---|---|
Moisture Absorption | 平衡,23°C,50%RH | ISO62 | 0.90 % |
Melt Volume flow Rate | 240°C/10.0kg | ISO1133 | 15.0 cm3/10min |
Modeling Shrinkage | ISO294-4 | 0.40 % |
Impact Properties | Test Condition | Test Method | BASF GERMANY/N NG-04 |
---|---|---|---|
Charpy Unnotched Impact Strength | 23°C | ISO179 | 30 kJ/m² |
-30°C | ISO179 | 25 kJ/m² |
Electrical Properties | Test Condition | Test Method | BASF GERMANY/N NG-04 |
---|---|---|---|
Volume Resistivity | IEC60093 | 1E+15 ohms·cm | |
Surface Resistivity | IEC60093 | 1E+14 ohms | |
Relative Permittivity | 1MHz | IEC60250 | 2.90 |
Dissipation Factor? | 1MHz | IEC60250 | 0.013 |
Contact Us
Get App
Top