Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPO GFN2 SABIC INNOVATIVE US
NORYL™
Household appliances,Household appliances,Fitness equipment,Automotive interior parts
enhance,Glass fiber reinforced, Glass fiber reinforced
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | SABIC INNOVATIVE US/GFN2 |
|---|---|---|---|
| Rockwell hardness | L-Sale | ASTM D785 | 106 |
| thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/GFN2 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed,3.20mm | ASTM D648 | 135 °C |
| 1.8MPa,Unannealed,6.40mm | ASTM D648 | 138 °C | |
| 0.45MPa,Unannealed,3.20mm | ASTM D648 | 141 °C | |
| 0.45MPa,Unannealed,6.40mm | ASTM D648 | 143 °C | |
| 0.45MPa,Unannealed,100mmSpan | ISO 75-2/Be | 143 °C | |
| 1.8MPa,Unannealed,100mmSpan | ISO 75-2/Ae | 137 °C | |
| Linear coefficient of thermal expansion | MD:-40to40°C | ASTME831 | 2.9E-05 cm/cm/°C |
| TD:-40to40°C | ASTME831 | 8.3E-05 cm/cm/°C | |
| RTI Elec | UL 746 | 90.0 °C | |
| RTI Imp | UL 746 | 90.0 °C | |
| RTI Str | UL 746 | 90.0 °C | |
| Vicat softening temperature | -- | ISO 306/B120 | 146 °C |
| -- | ISO 306/B50 | 143 °C |
| mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/GFN2 |
|---|---|---|---|
| Bending modulus | 50.0mmSpan | ASTM D790 | 5800 Mpa |
| ISO 178 | 6540 Mpa | ||
| bending strength | Yield,50.0mmSpan | ASTM D790 | 160 Mpa |
| ISO 178 | 167 Mpa | ||
| elongation | Break | ASTM D638 | 2.6 % |
| Tensile modulus | ISO 527-2/1 | 7070 Mpa | |
| ASTM D638 | 6200 Mpa | ||
| Tensile strain | Break | ISO 527-2/5 | 2.5 % |
| tensile strength | Break | ISO 527-2/5 | 97.3 Mpa |
| Break | ASTM D638 | 90.0 Mpa |
| Electrical performance | Test Condition | Test Method | SABIC INNOVATIVE US/GFN2 |
|---|---|---|---|
| Arc resistance | ASTM D495 | PLC7 | |
| Dielectric constant | 50Hz | ASTM D150 | 2.86 |
| 60Hz | ASTM D150 | 2.86 | |
| Dielectric strength | 3.20mm,inOil | ASTM D149 | 17 KV/mm |
| Dissipation factor | 60Hz | ASTM D150 | 8E-04 |
| 50Hz | ASTM D150 | 8E-04 | |
| High arc combustion index | HAI | UL 746 | PLC 4 |
| High voltage arc tracing rate | HVTR | UL 746 | PLC 4 |
| Hot wire ignition | HWI | UL 746 | PLC 4 |
| Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/GFN2 |
|---|---|---|---|
| density | ASTM D792 | 1.20 g/cm³ | |
| melt mass-flow rate | 300°C/5.0kg | ASTM D1238 | 9.0 g/10min |
| Melt Volume Flow Rate (MVR) | 300°C/5.0kg | ISO 1133 | 8.10 cm3/10min |
| Outdoor applicability | UL 746C | f1 | |
| Shrinkage rate | MD:3.20mm | Internal Method | 0.20-0.50 % |
| Water absorption rate | 24hr | ASTM D570 | 0.060 % |
| impact performance | Test Condition | Test Method | SABIC INNOVATIVE US/GFN2 |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/2C | 12 kJ/m² |
| Dart impact | 23°C,TotalEnergy | ASTM D3763 | 22.6 J |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 11 kJ/m² |
| 23°C | ASTM D256 | 120 J/m | |
| 23°C | ASTM D4812 | 650 J/m | |
| -40°C | ASTM D256 | 96 J/m |
| flammability | Test Condition | Test Method | SABIC INNOVATIVE US/GFN2 |
|---|---|---|---|
| Extreme Oxygen Index | ASTM D2863 | 26 % | |
| UL flame retardant rating | 1.5mm | UL 94 | HB |