PP TechnoFiber PP LGF 40-10-01 HI TECHNOCOMPOUND GERMANY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoFiber PP LGF 40-10-01 HI |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 20 kJ/m² |
-30°C | ISO 179/1eA | 21 kJ/m² | |
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 58 kJ/m² |
-30°C | ISO 179/1eU | 58 kJ/m² |
Mechanical properties | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoFiber PP LGF 40-10-01 HI |
---|---|---|---|
Flexural modulus | ISO 178 | 8900 MPa | |
Tensile modulus | ISO 527-2/1 | 8700 MPa | |
Tensile strain | 屈服 | ISO 527-2/50 | 2.5 % |
tensile strength | 屈服 | ISO 527-2/50 | 115 MPa |
bending strength | ISO 178 | 130 MPa |
physical property | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoFiber PP LGF 40-10-01 HI |
---|---|---|---|
Shrinkage rate | MD2 | ISO 294-4 | 0.20 % |
density | ISO 1183 | 1.20 g/cm³ |
Thermal performance | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoFiber PP LGF 40-10-01 HI |
---|---|---|---|
melting temperature | ISO 11357-3 | 165 °C | |
Linear coefficient of thermal expansion | TD:23到80°C | ISO 11359-2 | 3.4E-05 cm/cm/°C |
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 160 °C |
1.8MPa,未退火,HDT | ISO 75-2/A | 150 °C | |
Linear coefficient of thermal expansion | MD:23到80°C | ISO 11359-2 | 1.5E-05 cm/cm/°C |
Heat distortion temperature | 8.0MPa,未退火,HDT | ISO 75-2/C | 124 °C |