Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PBT 702MS JAPAN POLYPLASTIC
DURANEX®
Electrical applications,Electronic and electrical components
Flame retardant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Supplementary Information | Test Condition | Test Method | JAPAN POLYPLASTIC/702MS |
|---|---|---|---|
| ColourNumber | ED3002 |
| hardness | Test Condition | Test Method | JAPAN POLYPLASTIC/702MS |
|---|---|---|---|
| Rockwell hardness | M-Scale | ISO 2039-2 | 100 |
| thermal performance | Test Condition | Test Method | JAPAN POLYPLASTIC/702MS |
|---|---|---|---|
| Combustibility (rate) | UL 94 | HB | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 197 °C |
| 1.8Mpa | ISO 75-1/-2 | 197 °C | |
| Linear coefficient of thermal expansion | MD:23to55°C | Internal Method | 2E-05 cm/cm/°C |
| TD:23to55°C | Internal Method | 4E-05 cm/cm/°C | |
| UL flame retardant rating | UL 94 | HB |
| mechanical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/702MS |
|---|---|---|---|
| Bending modulus | ISO 178 | 15500 Mpa | |
| ASTM D790/ISO 178 | 15500 kg/cm²(MPa)[Lb/in²] | ||
| bending strength | ASTM D790/ISO 178 | 205 kg/cm²(MPa)[Lb/in²] | |
| ISO 178 | 205 Mpa | ||
| Charpy Notched Impact Strength | ISO 179/1eA | 6.5 KJ/m | |
| Elongation at Break | ASTM D638/ISO 527 | 1.3 % | |
| Tensile strain | Break | ISO 527-2 | 1.3 % |
| tensile strength | ISO 527-1/-2 | 153 Mpa | |
| ASTM D638/ISO 527 | 153 kg/cm²(MPa)[Lb/in²] | ||
| ISO 527-2 | 153 Mpa |
| Electrical performance | Test Condition | Test Method | JAPAN POLYPLASTIC/702MS |
|---|---|---|---|
| Volume resistivity | IEC 60093 | 6E+15 ohms·cm |
| Physical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/702MS |
|---|---|---|---|
| density | ASTM D792/ISO 1183 | 1.73 | |
| Water absorption rate | 23°C,24hr | ISO 62 | 0.10 % |
| flammability | Test Condition | Test Method | JAPAN POLYPLASTIC/702MS |
|---|---|---|---|
| UL flame retardant rating | UL 94 | HB |