Test Condition | Test Method | RESIRENE MEXICO/ 240 | |
---|---|---|---|
transmissivity | ASTM D1003 | 88.0 % | |
tensile strength | 断裂 | ASTM D638 | 22.0 MPa |
density | ASTM D792 | 1.05 g/cm³ | |
elongation | 断裂 | ASTM D638 | 45 % |
melt mass-flow rate | 200°C/5.0kg | ASTM D1238 | 7.0 g/10min |
Tensile modulus | ASTM D638 | 1900 MPa | |
UL flame retardant rating | 1.5mm | UL 94 | HB |
Impact strength of cantilever beam gap | 3.17mm | ASTM D256 | 21 J/m |
Suspended wall beam without notch impact strength | 3.18mm | ASTM D256 | 260 J/m |
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 70.0 °C |
vicat | ASTM D1525 | 72.0 °C |