PC/ABS MC8002-7001 SABIC INNOVATIVE JAPAN
CYCOLOY™
Automotive sector,Electrical field,Electronic field,Home appliance components,Application in the automotive field
heat-resisting
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | SABIC INNOVATIVE JAPAN/MC8002-7001 |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed,3.20mm | ASTM D648 | 107 °C |
1.8MPa,Unannealed,6.40mm | ASTM D648 | 110 °C | |
0.45MPa,Unannealed,3.20mm | ASTM D648 | 124 °C | |
Linear coefficient of thermal expansion | MD:-40to40°C | ASTME831 | 7.2E-05 cm/cm/°C |
thermal conductivity | ASTMC177 | 0.20 W/m/K |
mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE JAPAN/MC8002-7001 |
---|---|---|---|
Bending modulus | 50.0mmSpan | ASTM D790 | 2340 Mpa |
bending strength | Yield,50.0mmSpan | ASTM D790 | 86.2 Mpa |
elongation | Yield | ASTM D638 | 5.0 % |
Break | ASTM D638 | 150 % | |
Tensile modulus | ASTM D638 | 2210 Mpa | |
tensile strength | Yield | ASTM D638 | 56.5 Mpa |
Physical properties | Test Condition | Test Method | SABIC INNOVATIVE JAPAN/MC8002-7001 |
---|---|---|---|
melt mass-flow rate | 260°C/5.0kg | ASTM D1238 | 9.0 g/10min |
Shrinkage rate | MD:3.20mm | Internal Method | 0.50-0.70 % |
Water absorption rate | 24hr | ASTM D570 | 0.10 % |
Equilibrium,23°C | ASTM D570 | 0.40 % |
impact performance | Test Condition | Test Method | SABIC INNOVATIVE JAPAN/MC8002-7001 |
---|---|---|---|
Dart impact | -30°C,TotalEnergy | ASTM D3763 | 54.2 J |
23°C,TotalEnergy | ASTM D3763 | 61.0 J |