EVA Hanwha Total PE E282PV Hanwha Chemical
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | Hanwha Chemical/Hanwha Total PE E282PV |
|---|---|---|---|
| Shore hardness | ShoreD | ASTM D2240 | 22 |
| thermal performance | Test Condition | Test Method | Hanwha Chemical/Hanwha Total PE E282PV |
|---|---|---|---|
| Crystallization peak temperature | DSC | ASTM D3418 | 49.0 °C |
| Melting temperature | Internal Method | 70.0 °C | |
| Vicat softening temperature | ASTM D1525 | 38.0 °C |
| mechanical properties | Test Condition | Test Method | Hanwha Chemical/Hanwha Total PE E282PV |
|---|---|---|---|
| elongation | Break | ASTM D638 | 890 % |
| tensile strength | Break | ASTM D638 | 9.81 MPa |
| Physical properties | Test Condition | Test Method | Hanwha Chemical/Hanwha Total PE E282PV |
|---|---|---|---|
| density | ASTM D1505 | 0.948 g/cm³ | |
| melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 25 g/10min |
| Vinyl acetate content | Internal Method | 28.0 wt% |